Precautions when using furniture paper

(Summary description)Furniture paper can change the shape of the furniture.If wrinkles appear during the posting process,the overall furniture decoration effect will be affected.If you want to avoid wrinkles,

Precautions when using furniture paper

(Summary description)Furniture paper can change the shape of the furniture.If wrinkles appear during the posting process,the overall furniture decoration effect will be affected.If you want to avoid wrinkles,

  • Origin:
  • Time of issue:2020-05-06
Information
  Furniture paper can change the shape of the furniture.If wrinkles appear during the posting process,the overall furniture decoration effect will be affected.If you want to avoid wrinkles,you should make preparations before posting.In general,the base material used for stickers is mostly particleboard,and if the stickers are directly on the surface of these two boards,the stickers will often appear.The problem of unevenness,so the substrate must be treated to achieve smooth and smooth.
  Furniture paper,as the name implies,uses wood-grained paper veneer as the furniture base material.Wood grain paper veneer is different from solid wood and wood veneer,but it has the effect of wood grain.
  Generally speaking,paint stickers furniture should mainly pay attention to the following aspects:
  1.Treatment of substrates:Generally,the substrates used for stickers are mostly particleboard,and if the stickers are directly applied on the surface of these two boards,the problem of unevenness often occurs,so the substrate must be The wood is processed to make it smooth and smooth.For example,put a lot of water ash on the board,scrape putty,spray PU or PE solid color primer,etc.The advantage of a full batch of water ash is its low cost,and its disadvantage is mainly the problem of adhesion.Although putty solves the problem of adhesion to the substrate,we know that most of the putty on the market is single-component nitro putty,and from the perspective of the compatibility of paint,it is easily caused between the upper polyester thinner Bottom biting phenomenon in response.Spraying PU or PE solid color primer,the above problems will not occur.Therefore,it is currently the most popular.
  Second,the choice of paint:the effect of sticker furniture is good or bad,the first thing is to look at its transparency,followed by color,fullness,hardness,feel and so on.If the transparency of the paint is not good,it will directly affect the clarity and look of the color.Therefore,it is most important to choose a paint with good transparency.For example,primers,we can choose China Resources'PU-based PD3900,PD3300,PD3600,and PD1500 transparent primers and PE-based ED3100,ED3300,ED3600,and ED3900 transparent primers,etc.,while achieving high transparency and good filling power.,Fullness,hardness,yellowing resistance,sanding and other effects.For topcoats,we can choose China Resources'PU type P3600X,P3800X,P3400X and P2800X,and PE type ED3000,etc.,which not only ensure good transparency,but also meet the hardness,scratch resistance,fullness,feel and yellow resistance of the paint film.Equal requirements.
  Third,the coating process:the quality of the furniture is good or bad,the effect is not only dependent on the quality of the board.The quality of the paint,and choosing a reasonable coating process is also very important.In general,the process of painting sticker furniture can be divided according to the following procedures:
  1.White blank processing.Use 240#—320#sandpaper to eliminate surface stains and make the surface smooth.
  2.Closed.Closed with China Resources PS900 Depot and polished after 3-4 hours.
  3.Polishing.Lightly grind with 320#sandpaper to remove burr of wood wool.
  4.Primer.Spray China Resources PU or PE solid color primer to achieve a certain degree of fullness and hiding power,no bottom leakage,polish after 5-8 hours.
  5.Polishing.Polish thoroughly with 320#sandpaper,smooth and smooth.
  6.Stickers.Use wood grain paper,require stickers without bubbles,wrinkles,neat and consistent,after 24 hours of hard-coating primer.
  7.Primer.Spray China Resources PU or PE transparent primer to achieve a certain degree of fullness,polish it after 5-8 hours.
  8.Polishing.Use 400#—600#to polish smooth and smooth,no obvious sand marks and bright spots are required.
  9.Color correction.Mix CR Sina or Sesame with clear coat in proportion,spray it,and the color is required to be even and consistent.After 8-10 hours of hard drying,polish it.
  10.Polishing.Lightly grind with 800#—1000#sandpaper to remove surface particles.
  11.Cover light.Use China Resources Clearcoat,spray,require filtration,pay attention to dust,and dry it after 24 hours.
  The quality of furniture paper is good or bad.The transparency,color,fullness,hardness,feel,etc.all affect its explosion.You love it.After using good materials,it will be used after the corresponding process.There will be different effects.The quality of furniture and the effect are not only determined by the quality of the board.The quality of the paint,and choosing a reasonable coating process is also very important.

Contact Us

Shanzhuang Industrial Park, West Section of Jiefang Road, Linyi

Mobile version

xingmei

Message

Username used for comment:
客户留言
Description:
验证码

Copyright©Shandong Xingmei Decorative Material Co., Ltd.

Powered by  www.300.cn   鲁ICP备15042273号